Machine learning and atomic layer deposition: predicting saturation times from reactor growth profiles using artificial neural networks

2022-05-10 · Angel Yanguas-Gil, Jeffrey W. Elam

In this work we explore the application of deep neural networks to the optimization of atomic layer deposition processes based on thickness values obtained at different points of an ALD reactor. We introduce a dataset designed to train neural networks to predict saturation times based on the dose time and thickness values measured at different points of the reactor for a single experimental condition. We then explore different artificial neural network configurations, including depth (number of hidden layers) and size (number of neurons in each layers) to better understand the size and complexity that neural networks should have to achieve high predictive accuracy. The results obtained show that trained neural networks can accurately predict saturation times without requiring any prior information on the surface kinetics. This provides a viable approach to minimize the number of experiments required to optimize new ALD processes in a known reactor. However, the datasets and training procedure depend on the reactor geometry.

📄 PDF Abstract BibTeX arXiv:2205.08378

Code (1)

aldsim/saturationdataset 공식 구현 pytorch

Similar Papers 제목 키워드 기반

Surrogate models to optimize plasma assisted atomic layer deposition in high aspect ratio features

2025-06-11 · Angel Yanguas-Gil, Jeffrey W. Elam

In this work we explore surrogate models to optimize plasma enhanced atomic layer deposition (PEALD) in high aspect ratio features. In plasma-based processes such as PEALD and atomic layer etching, surface recombination …

On Simulating Thin-Film Processes at the Atomic Scale Using Machine Learned Force Fields

2025-05-02 · S. Kondati Natarajan, J. Schneider, N. Pandey, J. Wellendorff 외

Atomistic modeling of thin-film processes provides an avenue not only for discovering key chemical mechanisms of the processes but also to extract quantitative metrics on the events and reactions taking place at the gas-…

Publishing FAIR and Machine-actionable Reviews in Materials Science: The Case for Symbolic Knowledge in Neuro-symbolic Artificial Intelligence

2026-01-08 · Jennifer D'Souza, Soren Auer, Eleni Poupaki, Alex Watkins 외 arxiv

Scientific reviews are central to knowledge integration in materials science, yet their key insights remain locked in narrative text and static PDF tables, limiting reuse by humans and machines alike. This article presen…

Benchmarking large language models for materials synthesis: the case of atomic layer deposition

2024-12-13 · Angel Yanguas-Gil, Matthew T. Dearing, Jeffrey W. Elam, Jessica C. Jones 외

In this work we introduce an open-ended question benchmark, ALDbench, to evaluate the performance of large language models (LLMs) in materials synthesis, and in particular in the field of atomic layer deposition, a thin …

BenchmarkingHallucinationSpecificity

Performance of AI agents based on reasoning language models on ALD process optimization tasks

2026-01-15 · Angel Yanguas-Gil arxiv

In this work we explore the performance and behavior of reasoning large language models to autonomously optimize atomic layer deposition (ALD) processes. In the ALD process optimization task, an agent built on top of a r…